In Vivo Response of Growth Plate to Biodegradable Mg-Ca-Zn Alloys Depending on the Surface Modification

Full metadata record
DC Field Value Language
dc.contributor.authorSong, Mi Hyun-
dc.contributor.authorYoo, Won Joon-
dc.contributor.authorCho, Tae-Joon-
dc.contributor.authorPark, Yong Koo-
dc.contributor.authorLee, Wang-Jae-
dc.contributor.authorChoi, In Ho-
dc.date.available2020-11-02T06:34:08Z-
dc.date.issued2019-08-
dc.identifier.issn1422-0067-
dc.identifier.urihttps://scholarworks.korea.ac.kr/kumedicine/handle/2020.sw.kumedicine/1778-
dc.description.abstractBecause Mg-Ca-Zn alloys are biodegradable and obviate secondary implant removal, they are especially beneficial for pediatric patients. We examined the degradation performance of Mg-Ca-Zn alloys depending on the surface modification and investigated the in vivo effects on the growth plate in a skeletally immature rabbit model. Either plasma electrolyte oxidation (PEO)-coated (n = 18) or non-coated (n = 18) Mg-Ca-Zn alloy was inserted at the distal femoral physis. We measured the degradation performance and femoral segment lengths using micro-CT. In addition, we analyzed the histomorphometric and histopathologic characteristics of the growth plate. Although there were no acute, chronic inflammatory reactions in either group, they differed significantly in the tissue reactions to their degradation performance and physeal responses. Compared to non-coated alloys, PEO-coated alloys degraded significantly slowly with diminished hydrogen gas formation. Depending on the degradation rate, large bone bridge formation and premature physeal arrest occurred primarily in the non-coated group, whereas only a small-sized bone bridge formed in the PEO-coated group. This difference ultimately led to significant shortening of the femoral segment in the non-coated group. This study suggests that optimal degradation could be achieved with PEO-coated Mg-Ca-Zn alloys, making them promising and safe biodegradable materials with no growth plate damage.-
dc.language영어-
dc.language.isoENG-
dc.publisherMultidisciplinary Digital Publishing Institute (MDPI)-
dc.titleIn Vivo Response of Growth Plate to Biodegradable Mg-Ca-Zn Alloys Depending on the Surface Modification-
dc.typeArticle-
dc.publisher.location스위스-
dc.identifier.doi10.3390/ijms20153761-
dc.identifier.scopusid2-s2.0-85070952199-
dc.identifier.wosid000482383000154-
dc.identifier.bibliographicCitationInternational Journal of Molecular Sciences, v.20, no.15-
dc.citation.titleInternational Journal of Molecular Sciences-
dc.citation.volume20-
dc.citation.number15-
dc.type.docTypeArticle-
dc.description.isOpenAccessY-
dc.description.journalRegisteredClassscie-
dc.description.journalRegisteredClassscopus-
dc.relation.journalResearchAreaBiochemistry & Molecular Biology-
dc.relation.journalResearchAreaChemistry-
dc.relation.journalWebOfScienceCategoryBiochemistry & Molecular Biology-
dc.relation.journalWebOfScienceCategoryChemistry, Multidisciplinary-
dc.subject.keywordPlusMAGNESIUM ALLOYS-
dc.subject.keywordPlusDEGRADATION-
dc.subject.keywordPlusBIOACTIVITY-
dc.subject.keywordPlusCORROSION-
dc.subject.keywordPlusVITRO-
dc.subject.keywordPlusMECHANISM-
dc.subject.keywordPlusRESECTION-
dc.subject.keywordPlusCOATINGS-
dc.subject.keywordPlusRABBIT-
dc.subject.keywordAuthorbiodegradable-
dc.subject.keywordAuthorMg-Ca-Zn alloy-
dc.subject.keywordAuthorplasma electrolyte oxidation-
dc.subject.keywordAuthorgrowth plate-
Files in This Item
There are no files associated with this item.
Appears in
Collections
2. Clinical Science > Department of Orthopedic Surgery > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Altmetrics

Total Views & Downloads

BROWSE